SGQ 5.88% 3.6¢ st george mining limited

Mixed grinding with Na2S followed by water leaching was...

  1. 1,047 Posts.
    lightbulb Created with Sketch. 112
    Mixed grinding with Na2S followed by water leaching was performed to extract Li from lepidolite. The leachability of Li increases dramatically in the ground mixture, regardless of the mixing ratio over the range of 1:1 to 3:1, while only 4.53% of Li was extracted in lepidolite ground without Na2S. The leachability increased with an increase of the grinding time, and ultimately, 93% of the Li was leached by water from the ground mixture with a weight ratio of 3:1 (Na2S:Lepidolite). In the process of the mixed grinding, the Li-contained lepidolite was destructured crystallographically, and it might have changed to different compounds. This process enables us to extract Li from lepidolite via a water leaching treatment.


 
watchlist Created with Sketch. Add SGQ (ASX) to my watchlist
(20min delay)
Last
3.6¢
Change
0.002(5.88%)
Mkt cap ! $39.18M
Open High Low Value Volume
3.5¢ 3.7¢ 3.5¢ $271.7K 7.731M

Buyers (Bids)

No. Vol. Price($)
4 1614600 3.5¢
 

Sellers (Offers)

Price($) Vol. No.
3.6¢ 418130 4
View Market Depth
Last trade - 16.10pm 26/08/2024 (20 minute delay) ?
SGQ (ASX) Chart
arrow-down-2 Created with Sketch. arrow-down-2 Created with Sketch.